Normal
I would grind that weld down flush, drill a hole in end of crack. Weld up crack, regrind flush again. Then weld a lap plate over joint, one on both sides if possible, (if both sides stagger where welds are to limit heat). If you want even more ruggedness, drill some holes in the lap plate & plug weld them also.